Material Notes:
HyTemp AR715 contains acrylic esters with a small percentage of a chlorine reactive cure site monomer. Vulcanizates have excellent oil, heat, and compression set resistance.Improved low-temperature and excellent oil resistance.
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
Mooney Viscosity 27 - 39

@Temperature 100 °C
27 - 39

@Temperature 212 °F
(1+4); Zeon Test #404
Ash <= 0.50 %
<= 0.50 %
Zeon Test #873
Thermal Properties Metric English Comments
Minimum Service Temperature, Air -24.0 °C
-11.2 °F
Gehman T100
Glass Transition Temp, Tg -20.9 - -12.9 °C
-5.62 - 8.78 °F
Zeon Test #1273
Descriptive Properties Value Comments
% Volume Swell 15
Curesite Chlorine
Gel-Mek (%), max 10
Heat Loss (%) Max 0.7