Minimum Service Temperature, Air -24.0 °C
-11.2 °F
Torsion Stiffness Temperature
Stir SpA Giesse EPM/78 (PVC)
Application: Extrusion medical parts - medium flexibilityInformation provided by STIR SpA
Minimum Service Temperature, Air -24.0 °C
-11.2 °F
Torsion Stiffness Temperature
Stir SpA Giesse EPM/81 (PVC)
Application: Extrusion medical parts - medium flexibilityInformation provided by STIR SpA
Minimum Service Temperature, Air -24.0 °C
-11.2 °F
Torsion Stiffness Temperature
Stir SpA Giesse IPM/6Z (PVC)
Application: Molding little parts - high flexibilityInformation provided by STIR SpA
Minimum Service Temperature, Air -24.0 °C
-11.2 °F
Gehman T100
Zeon Chemicals HyTemp® AR715 AR Polyacrylate Elastomer
HyTemp AR715 contains acrylic esters with a small percentage of a chlorine reactive cure site monomer. Vulcanizates have excellent oil, heat, and compression set resistance.Improved low-temperature ..
Minimum Service Temperature, Air -24.0 °C
-11.2 °F
JIS-K-6723
Denka VINYKON W4200 PVC, W grade for equipment cords, for heat resistance
A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding..
Minimum Service Temperature, Air -24.0 °C
-11.2 °F
JIS-K-6723
Denka VINYKON W1025 PVC, W grade for insulation, for sheaths
A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding..