Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | -20.9 - -12.9 °C | -5.62 - 8.78 °F | Zeon Test #1273 |
Zeon Chemicals HyTemp® AR715 AR Polyacrylate Elastomer HyTemp AR715 contains acrylic esters with a small percentage of a chlorine reactive cure site monomer. Vulcanizates have excellent oil, heat, and compression set resistance.Improved low-temperature .. |