Material Notes:
All-purpose alloy for low-fusing high expanding ceramicsApplications: inlays/onlays, crowns, short span bridges, long span bridges, telescopic and milling works, removable partials, ceramic veneering, acrylic veneeringDental
Physical Properties Metric English Comments
Density 10.6 g/cc
0.383 lb/in³
Mechanical Properties Metric English Comments
Hardness, Vickers 220
220
HV5/30; after porcelain firing
240
240
HV5/30; hardened
Tensile Strength, Yield 450.00 MPa

@Strain 0.200 %
65267 psi

@Strain 0.200 %
after porcelain firing
470.00 MPa

@Strain 0.200 %
68168 psi

@Strain 0.200 %
hardened
Elongation at Break 10 %
10 %
hardened
11 %
11 %
after porcelain firing
Modulus of Elasticity 95.0 GPa
13800 ksi
Thermal Properties Metric English Comments
CTE, linear 16.2 µm/m-°C

@Temperature 25.0 - 500 °C
9.00 µin/in-°F

@Temperature 77.0 - 932 °F
Component Elements Properties Metric English Comments
Indium, In 1.3 %
1.3 %
Palladium, Pd 39 %
39 %
Silver, Ag 54.7 %
54.7 %
Tin, Sn 2.0 %
2.0 %
Zinc, Zn 3.0 %
3.0 %
Processing Properties Metric English Comments
Processing Temperature 850.0 °C
1562 °F
Preheating Temp.
Melt Temperature 1100 - 1170 °C
2012 - 2138 °F
Casting Temperature 1300 °C
2372 °F
Descriptive Properties Value Comments
Color white