Mechanical Properties Metric English Comments
Tensile Strength, Yield 529.9 MPa

@Strain 0.200 %
76850 psi

@Strain 0.200 %
hardened
Wieland Euro 50 PFM Alloy
Gold-palladium ceramic alloyApplications: crowns, short span bridges, long span bridges, telescopic and milling work, ceramic veneering, acrylic veneeringDental