Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 114 GPa | 16500 ksi | |
Meehanite GC-40 Flake Graphite Cast Iron Type GC-40 combines good strength with low coefficient of friction and self lubricating properties. It is easily machinable with a fine, dense, close grain structure. Recommended for heavy brake d.. |
|||
Modulus of Elasticity | 114 GPa | 16500 ksi | |
Schott N-LASF43 Glass Information Provided by SCHOTT North America, Inc. |
|||
Modulus of Elasticity | 114 GPa | 16500 ksi | |
Wieland Euro 50 PFM Alloy Gold-palladium ceramic alloyApplications: crowns, short span bridges, long span bridges, telescopic and milling work, ceramic veneering, acrylic veneeringDental |
|||
Modulus of Elasticity | 114 GPa | 16500 ksi | Plate |
CMW® 3 Copper Alloy CMW® 3 material is a high strength, high conductivity copper base alloy. CMW® 3 material is heat treatable. Optimum mechanical and physical properties of CMW® 3 material are developed by heat tre.. |
|||
Modulus of Elasticity | 114 GPa | 16500 ksi | |
CMW® 353 Copper Alloy CMW® 353 material is an economical high strength, high conductivity copper base alloy. It is a heat treatable copper base alloy and its excellent properties are obtained largely through heat treatm.. |
|||
Modulus of Elasticity | 114 GPa | 16500 ksi | Long. |
ATI Wah Chang 425™ Titanium Alloy, Hot Rolled & Annealed Plate ATI 425™ titanium is an innovative high strength alloy that has strength comparable to Ti-6-4, yet has the advantage that it can be cold worked. Originally developed for armor plate for ballistic p.. |