Westlake Epolene® E-14P Oxidized Low Molecular Weight Polyethylene Polymer

Category Polymer , Thermoplastic , Polyethylene (PE)
Manufacturer Westlake Chemical Corporation
Trade Name Epolene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Westlake Epolene® E-14P Oxidized Low Molecular Weight Polyethylene Polymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: The Epolene E-14P is a low molecular-weight, low-density, oxidized polyethylene powder. It is useful as a lubricant in processing rigid and flexible polyvinyl chloride (PVC) and as a processing aid for preparing color concentrates. Epolene E-14P is listed with the National Sanitation Foundation (NSF) under Standard 61 Drinking Water System Components Health Effects.Key Attributes:Imparts slip resistance, durability, and toughness to floor finishesListed with NSF for use as a lubricant in PVC melt processesLow density polyethylene (PE)Oxidized to provide functionalityProduces stable water based emulsionsApplication/Uses:Automotive OEMAutomotiveBuilding and ConstructionHot Melt AdhesivesPressure Sensitive AdhesivesSolventborne AdhesivesWaterborne AdhesivesWax ModificationInformation provided by Westlake Chemical
Physical Properties Metric English Comments
Specific Gravity 0.930 - 0.960 g/cc
0.930 - 0.960 g/cc
Viscosity 300 - 400 cP

@Temperature 125 °C
300 - 400 cP

@Temperature 257 °F
TXAL-A-XX-G-V-005
Brookfield Viscosity 375 cP

@Temperature 125 °C
375 cP

@Temperature 257 °F
Molecular Weight 4000 g/mol
4000 g/mol
Thermal Properties Metric English Comments
Flash Point >= 204 °C
>= 399 °F
Ring & Ball Softening Point 104 °C
219 °F
ASTM E28
Optical Properties Metric English Comments
Gardner Color Number <= 3.0
<= 3.0
TXAL-A-XX-G-VCC-99
Chemical Properties Metric English Comments
Total Acid Number 17
17
mg KOH/g
Descriptive Properties Value Comments
Penetration Hardness 4 dmm
ASTM D5, Needle under 100-g load for 5s @ 25 °C