Westlake Elevate™ DA528AA Ethylene Vinyl Acetate Copolymer

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate
Manufacturer Westlake Chemical Corporation
Trade Name Elevate™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Westlake Elevate™ DA528AA Ethylene Vinyl Acetate Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Developmental ProductDescription: Westlake ELEVATE™ DA528 is an ethylene vinyl acetate copolymer with 18.5% VA. DA528 is designed for blown and cast films requiring excellent optics and low heat seal initiation. High melt strength makes DA528 an excellent choice for profile extrusions, molding, and foaming applications requiring high VA content.Application/Uses:Flexible packaging filmsPeelable seals, adhesive layersInjection and blow moldingHot melt adhesives and blendsProfile extrusions, tubing, wire & cableInformation provided by Westlake Chemical
Physical Properties Metric English Comments
Density 0.940 g/cc
0.0340 lb/in³
ASTM D1505
Melt Flow 2.5 g/10 min
2.5 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Dart Drop Test 390 g
0.860 lb
ASTM D1709
Film Tensile Strength at Break, MD 24.8 MPa
3600 psi
ASTM D882
Film Tensile Strength at Break, TD 24.1 MPa
3500 psi
ASTM D882
1% Secant Modulus, MD 42.1 MPa
6100 psi
ASTM D882
1% Secant Modulus, TD 50.3 MPa
7300 psi
ASTM D882
Thermal Properties Metric English Comments
Melting Point 85.0 °C
185 °F
Peak, by DSC; ASTM D3418
Flash Point >= 343 °C
>= 649 °F
ASTM E136
Optical Properties Metric English Comments
Haze 3.5 %
3.5 %
ASTM D1003
Gloss 82 %
82 %
@ 45°; ASTM D2457