Thermal Properties Metric English Comments
Flash Point >= 343 °C
>= 649 °F
ASTM E136
Westlake Elevate™ DA528AA Ethylene Vinyl Acetate Copolymer
Developmental ProductDescription: Westlake ELEVATE™ DA528 is an ethylene vinyl acetate copolymer with 18.5% VA. DA528 is designed for blown and cast films requiring excellent optics and low heat s..
Flash Point >= 343 °C
>= 649 °F
ASTM E136
Westlake Elevate™ DA532 Ethylene Vinyl Acetate Copolymer
Experimental ProductDescription: Westlake DA532 resin is a 12.0% EVA copolymer designed for use as a sealant / lamination layer in monolayer or coextruded flexible film structures. It has very low ..
Flash Point >= 343 °C
>= 649 °F
ASTM E136
Westlake Epolene® C-10 Coating Grade - Highly Branched Medium Molecular Weight Polyethylene Polymer
Product Description: Epolene C-10 is a branched low density polyethylene homopolymer with low color and medium molecular weight. It is useful as a base polymer for adhesives and coatings, color conc..
Flash Point >= 343 °C
>= 649 °F
ASTM E136
Westlake Epolene® C-13 Coating Grade - Highly Branched Medium Molecular Weight Polyethylene Polymer
Product Description: Epolene C-13 is a branched low density polyethylene homopolymer with low color and medium molecular weight. It is useful as a base polymer for adhesives and coatings, color conc..
Flash Point >= 343 °C
>= 649 °F
ASTM E136
Westlake Epolene® C-13P Coating Grade - Branched Medium Molecular Weight Polyethylene Polymer
Description: Epolene C-13P is a branched low density polyethylene homopolymer powder with low color and medium molecular weight. It is useful as a base polymer for adhesives and coatings, color con..
Flash Point >= 343 °C
>= 649 °F
ASTM E136
Westlake Epolene® C-15 Coating Grade - Highly Branched Medium Molecular Weight Polyethylene Polymer
Product Description: Epolene C-15 is a branched low density polyethylene homopolymer with low color and medium molecular weight. It is useful as a base polymer for adhesives and coatings, color conc..
Flash Point >= 343 °C
>= 649 °F
ASTM E136
Westlake Epolene® C-15P Coating Grade - Branched Medium Molecular Weight Polyethylene Polymer
Description: Epolene C-15P is a branched low density polyethylene homopolymer powder with low color and medium molecular weight. It is useful as a base polymer for adhesives and coatings, color conc..
Flash Point >= 343 °C
>= 649 °F
ASTM E136
Westlake Epolene® C-17 Coating Grade - Highly Branched Medium Molecular Weight Polyethylene Polymer
Product Description: Epolene C-17 is a branched low density polyethylene with a relatively high melt point and viscosity compared to other Epolene C-type Polymers. It is useful to modify paraffin wa..
Flash Point >= 343 °C
>= 649 °F
ASTM E136
Westlake Epolene® C-17P Coating Grade - Branched Medium Molecular Weight Polyethylene Polymer
Description: Epolene C-17P is a branched low density polyethylene powder with a relatively high melt point and viscosity compared to other Epolene C-type Polymers. It is useful to modify paraffin wa..
Flash Point >= 343 °C
>= 649 °F
ASTM E136
Westlake Epolene® L630-29L Branched Low Density Polyethylene Homopolymer
Description: Epolene L-630-29P is a branched low density polyethylene homopolymer powder with low color and medium molecular weight. It is useful as a base polymer for adhesives and coatings, color ..
Flash Point >= 343 °C
>= 649 °F
ASTM E136
Westlake Epolene® N-10 Nonemulsifiable - Low Molecular Weight Polyethylene Polymer
Product Description: Epolene N-10 is a polyethylene (PE) homopolymer that can easily be melt blended with natural or synthetic waxes to increase the tensile strength of wax blends, improve the gloss..
Flash Point >= 343 °C
>= 649 °F
ASTM E136
Westlake Epolene® N-11P Nonemulsifiable - Low Molecular Weight Polyethylene Polymer
Information provided by Westlake Chemical
Flash Point >= 343 °C
>= 649 °F
ASTM E136
Westlake Epolene® N-14 Nonemulsifiable - Low Molecular Weight Polyethylene Polymer
Product Description: Epolene N-14 is a polyethylene (PE) homopolymer that can easily be melt blended with natural or synthetic waxes to increase the tensile strength of wax blends, improve the gloss..
Flash Point >= 343 °C
>= 649 °F
ASTM E136
Westlake Epolene® N-14P Nonemulsifiable - Low Molecular Weight Polyethylene Polymer
Description: Epolene N-14P is a polyethylene (PE) homopolymer powder that can easily be melt blended with natural or synthetic waxes to increase the tensile strength of wax blends, improve the gloss..
Flash Point >= 343 °C
>= 649 °F
ASTM E136
Westlake Epolene® N-21 Nonemulsifiable - Low Molecular Weight Polyethylene Polymer
Product Description: Epolene N-21 is a medium density polyethylene that improves slump resistance in cable filling and flooding, provides lubricity in printing inks, and can be used as a viscosity m..
Flash Point >= 343 °C
>= 649 °F
ASTM E136
Westlake Epolene® N-21P Nonemulsifiable - Low Molecular Weight Polyethylene Polymer
Description: Epolene N-21P is a medium density polyethylene that improves slump resistance in cable filling and flooding, provides lubricity in printing inks, and can be used as a viscosity modifier..
Flash Point >= 343 °C
>= 649 °F
ASTM E136
Westlake Epolene® N-30 Nonemulsifiable - Low Molecular Weight Polyethylene Polymer
Product Description: Epolene N-30 is a polyethylene (PE) homopolymer that can easily be melt blended with natural or synthetic waxes to increase the tensile strength of wax blends, improve the gloss..
Flash Point >= 343 °C
>= 649 °F
ASTM E136
Westlake Epolene® N-34 Nonemulsifiable - Low Molecular Weight Polyethylene Polymer
Product Description: Epolene N-34 is a polyethylene (PE) homopolymer that can easily be melt blended with natural or synthetic waxes to increase the tensile strength of wax blends, improve the gloss..
Flash Point >= 343 °C
>= 649 °F
ASTM E136
Westlake Epolene® N-34P Nonemulsifiable - Low Molecular Weight Polyethylene Polymer
Description: Epolene N-34P is a polyethylene (PE) homopolymer powder that can easily be melt blended with natural or synthetic waxes to increase the tensile strength of wax blends, improve the gloss..
Flash Point >= 343 °C
>= 649 °F
ASTM E136
Westlake Epolene® N-35 Nonemulsifiable - Low Molecular Weight Polyethylene Polymer
Product Description: Epolene N-35 is a polyethylene (PE) homopolymer that can easily be melt blended with natural or synthetic waxes to increase the tensile strength of wax blends, improve the gloss..
Flash Point >= 343 °C
>= 649 °F
ASTM E136
Westlake Epolene® N-11 Nonemulsifiable - Low Molecular Weight Polyethylene Polymer
Product Description: Epolene N-11 is a polyethylene (PE) homopolymer that can easily be melt blended with natural or synthetic waxes to increase the tensile strength of wax blends, improve the gloss..
Copyright © lookpolymers.com All Rights Reserved