Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, MD | 42.1 MPa | 6100 psi | ASTM D882 |
Westlake Elevate™ DA528AA 18.5% Ethylene Vinyl Acetate Copolymer Westlake ELEVATE™ DA528 is an ethylene vinyl acetate copolymer with 18.5% VA. DA528 is designed for blown and
cast films requiring excellent optics and low heat seal initiation. High melt strength.. |
|||
1% Secant Modulus, MD | 42.1 MPa | 6100 psi | ASTM D882 |
Westlake Elevate™ DA528AA Ethylene Vinyl Acetate Copolymer Developmental ProductDescription: Westlake ELEVATE™ DA528 is an ethylene vinyl acetate copolymer with 18.5% VA. DA528 is designed for blown and cast films requiring excellent optics and low heat s.. |