Westlake EC812AA Low Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE
Manufacturer Westlake Chemical Corporation
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Westlake EC812AA Low Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
WESTLAKE low-density polyethylene EC812 is a natural low-density material with a 200 melt index. Its high melt index exhibits excellent wettability. This makes it ideal as a backing to carpet to bind the fibers to the carpet.Application/UsesFlexible medicalMedicalFDA: This material complies with FDA regulations in 21 CFR, section 177.1520. Kosher Compliant.All information provided by Westlake Chemical
Physical Properties Metric English Comments
Density 0.909 g/cc
0.0328 lb/in³
ASTM D1505
Melt Flow 200 g/10 min

@Load 2.16 kg,
Temperature 190 °C
200 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 6.20 MPa
899 psi
500mm/min; ASTM D638 Type IV Specimen
Elongation at Break 100 %
100 %
500mm/min; ASTM D638 Type IV Specimen
2% Secant Modulus 0.103 GPa
14.9 ksi
12.7mm/min; ASTM D790
Processing Properties Metric English Comments
Melt Temperature 149 - 166 °C
300 - 330 °F
Descriptive Properties Value Comments
Process Coating