Wellman Wellamid® T512-BK 15% Talc/Glass Reinforced, Dimensionally Stable Grade Nylon 6

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Glass/Mineral Reinforced
Manufacturer Wellman Engineering Resins
Trade Name Wellamid®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wellman Wellamid® T512-BK 15% Talc/Glass Reinforced, Dimensionally Stable Grade Nylon 6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Talc/Glass Reinforced, Dimensionally Stable Grade Nylon 6Information provided by Wellman.
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
ISO 1183-87
Filler Content 15 %
15 %
Linear Mold Shrinkage, Flow 0.0075 - 0.0105 cm/cm
0.0075 - 0.0105 in/in
ISO DIS 294-4
Linear Mold Shrinkage, Transverse 0.0075 - 0.0105 cm/cm
0.0075 - 0.0105 in/in
ISO DIS 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 80.0 MPa
11600 psi
ISO 527-93
Elongation at Break 2.5 %
2.5 %
ISO 527-93
Flexural Strength 110 MPa
16000 psi
ISO 178-93
Flexural Modulus 4.20 GPa
609 ksi
ISO 178-93
Izod Impact, Notched (ISO) 3.00 kJ/m²
1.43 ft-lb/in²
ISO 180-93
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 160 °C
320 °F
ISO 75-93