Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Vicone High Performance Rubber VicoSil™ KC605Q-OR High Performance Silicone Rubber

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber
Manufacturer Vicone High Performance Rubber
Trade Name VicoSil™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Vicone High Performance Rubber VicoSil™ KC605Q-OR High Performance Silicone Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Vicone
Physical Properties Metric English Comments
Density 1.166 g/cc
0.04212 lb/in³
ASTM D3165
Mechanical Properties Metric English Comments
Hardness, Shore D 54
54
ASTM D2240
59.022

@Treatment Temp. 200 °C,
Time 252000 sec
59.022

@Treatment Temp. 392 °F,
Time 70.0 hour
Heat Aging; ASTM D573
Tensile Strength, Yield 8.00 MPa
1160 psi
ASTM D412
6.304 MPa

@Treatment Temp. 200 °C,
Time 252000 sec
914.3 psi

@Treatment Temp. 392 °F,
Time 70.0 hour
Heat Aging; ASTM D573
Elongation at Break 551.6 %
551.6 %
ASTM D412
345.85 %

@Treatment Temp. 200 °C,
Time 252000 sec
345.85 %

@Treatment Temp. 392 °F,
Time 70.0 hour
Heat Aging; ASTM D573
Compressive Modulus 0.000390 GPa

@Strain 5.00 %
0.0566 ksi

@Strain 5.00 %
0.000710 GPa

@Strain 10.0 %
0.103 ksi

@Strain 10.0 %
0.00140 GPa

@Strain 20.0 %
0.203 ksi

@Strain 20.0 %
0.00174 GPa

@Strain 25.0 %
0.252 ksi

@Strain 25.0 %
Compression Set 6.43 %

@Temperature 175 °C,
Time 79200 sec
6.43 %

@Temperature 347 °F,
Time 22.0 hour
ASTM D395
Descriptive Properties Value Comments
Color Orange