Universal Wire Works ER316L Stainless Steel Bare Wire

Category Metal , Ferrous Metal , Stainless Steel
Manufacturer Universal Wire Works
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Universal Wire Works ER316L Stainless Steel Bare Wire.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This alloy is the same as ER316, except that the carbon content has been restricted. Low (0.03% maximum) carbon in this filler metal reduces the possibility of intergranular chromium carbide precipitation thus increases the resistance to intergranular corrosion without the use of stabilizers such as columbium or titanium. ER316L is primarily used for welding low carbon molybdenum bearing austenitic stainless steels. The low carbon 316L is not as strong at elevated temperatures as the stabilized alloys or ER316H.Information provided by Universal Wire Works for their line of welding wire and filler metal.
Component Elements Properties Metric English Comments
Carbon, C 0.00 - 0.030 %
0.00 - 0.030 %
Chromium, Cr 19 %
19 %
Iron, Fe 69.5 - 69.5 %
69.5 - 69.5 %
As Remainder
Molybdenum, Mo 2.5 %
2.5 %
Nickel, Ni 9.0 %
9.0 %