Shinkong Synthetic Fibers Shinite® N601G30 Nylon 66, 30% Glass Filled

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled
Manufacturer Shinkong Synthetic Fibers Corp
Trade Name Shinite®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shinkong Synthetic Fibers Shinite® N601G30 Nylon 66, 30% Glass Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information from Shinkong Synthetic Fibers Corp.
Physical Properties Metric English Comments
Specific Gravity 1.40 g/cc
1.40 g/cc
ASTM D792
Water Absorption 0.60 %
0.60 %
ASTM D570
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
ASTM D955
Linear Mold Shrinkage, Transverse 0.012 - 0.015 cm/cm
0.012 - 0.015 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength 186 MPa
27000 psi
ASTM D638
Elongation at Break 5.0 %
5.0 %
ASTM D638
Flexural Yield Strength 284 MPa
41200 psi
ASTM D790
Flexural Modulus 9.81 GPa
1420 ksi
ASTM D790
Izod Impact, Notched 1.18 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
2.20 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 230 °C
446 °F
ASTM D648
Flammability, UL94 HB
HB