Universal Wire Works 502 E8018-B6 Stainless Steel Electrode

Category Metal , Ferrous Metal , Stainless Steel
Manufacturer Universal Wire Works
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Universal Wire Works 502 E8018-B6 Stainless Steel Electrode.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Universal 502 electrodes are used for the welding of types 501 and 502 straight chromium steels. Principal applications are in the fabrication of equipment for the oil and chemical industries where service conditions require resistance to corrosion and oxidation at elevated temperatures. Alloy 502 is an air hardening alloy requiring a preheat and postweld heat treatment.Information provided by Universal Wire Works for their line of welding wire and filler metal.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 565 MPa
82000 psi
Elongation at Break 30 %
30 %
Component Elements Properties Metric English Comments
Carbon, C 0.10 %
0.10 %
Chromium, Cr 5.0 %
5.0 %
Iron, Fe 94.4 %
94.4 %
As Remainder
Molybdenum, Mo 0.50 %
0.50 %