Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 565 MPa
82000 psi
Universal Wire Works 410 Stainless Steel Electrode
Universal 410 is a 12% straight chromium electrode used for the welding of type 410 stainless steel in the fabrication of equipment that demands corrosion resistance, good strength and ductility. Al..
Tensile Strength, Ultimate 565 MPa
82000 psi
Universal Wire Works 502 E8018-B6 Stainless Steel Electrode
Universal 502 electrodes are used for the welding of types 501 and 502 straight chromium steels. Principal applications are in the fabrication of equipment for the oil and chemical industries where ..
Tensile Strength, Ultimate 565 - 621 MPa
82000 - 90000 psi
Eagle Brass 230 Red Brass, Extra Spring
CDA 230 is known for having an electrical conductivity of 37% IACS, red color, corrosion resistance, excellent formability and moderate strength. Typical uses include costume jewelry, eyelets, faste..