Formosa Plastics Formolene® 4100P Injection Molding Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Formosa Plastics Corporation, USA
Trade Name Formolene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Formosa Plastics Formolene® 4100P Injection Molding Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Homopolymer with ESCR AdditivesApplications: Closures, small appliances, housewares and toys.Formolene 4100P is a low viscosity, highly isotactic polypropylene homopolymer designed for various injection molded applications such as closures, small appliances, housewares and toys. It contains a unique combination of stabilizers which give it excellent processability with good stiffness, environmental stress crack resistance, heat performance and minimal odor and taste.Meets all requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, covering safe use of polyolefin articles intended for direct food contact.Specimens were injection molded according to the conditions specified in ASTM D4101.Information provided by Formosa Plastics Corporation, USA.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 20 g/10 min

@Temperature 230 °C
20 g/10 min

@Temperature 446 °F
I<sub>2</sub>; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 105
105
ASTM D785
Tensile Strength, Yield 33.8 MPa
4900 psi
2" (50mm) per min.; ASTM D638
Elongation at Yield 8.0 %
8.0 %
2" (50mm) per min.; ASTM D638
Flexural Modulus 1.24 GPa
180 ksi
1.3mm per min, 1% secant; ASTM D790
Izod Impact, Notched 0.267 J/cm
0.500 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 100 °C
212 °F
ASTM D648