Material Notes:
Production Method: Waste diesel oil is produced when diesel oil is used a cracked gas cooling or flushing agent in the process of ethylene production. Application: Waste diesel oil is shipped to petroleum storage and exported.Information Provided by Kazanorgsintez
Physical Properties Metric English Comments
Density >= 0.900 g/cc

@Temperature 19.0 - 20.0 °C
>= 0.0325 lb/in³

@Temperature 66.2 - 68.0 °F
Kinematic Viscosity <= 12 cSt

@Temperature 49.9 - 50.1 °C
<= 12 cSt

@Temperature 122 - 122 °F
Ash <= 0.20 %
<= 0.20 %
Thermal Properties Metric English Comments
Pour Point <= -10.0 °C
<= 14.0 °F
Flash Point >= 45.0 °C
>= 113 °F
determined in closed gap
Component Elements Properties Metric English Comments
Free Water <= 1.0 %
<= 1.0 %
Sulfur, S <= 0.50 %
<= 0.50 %
Descriptive Properties Value Comments
Amount of impurities [pcs] 1
Mechanical impurities