Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 20000 g/mol | 20000 g/mol | |
Unitika elitel UE3201 Polyester, Pellet High molecular weight type UE3200UNITIKA l resins are thermoplastic saturated copolymeric polyester resins. l resins are expanding their applications from products such as adhesives, paints, ink bi.. |
|||
Molecular Weight | 20000 g/mol | 20000 g/mol | |
Unitika elitel UE3203 Polyester, Pellet High elongation type UE3200UNITIKA l resins are thermoplastic saturated copolymeric polyester resins. l resins are expanding their applications from products such as adhesives, paints, ink binders,.. |
|||
Molecular Weight | 20000 g/mol | 20000 g/mol | |
Unitika elitel UE3210 Polyester, Pellet Medium Tg, standard resin, BinderUNITIKA l resins are thermoplastic saturated copolymeric polyester resins. l resins are expanding their applications from products such as adhesives, paints, ink bi.. |
|||
Molecular Weight | 20000 g/mol | 20000 g/mol | |
Unitika elitel UE3230 Polyester, Flake Adhesive agent, Resin modifierUNITIKA l resins are thermoplastic saturated copolymeric polyester resins. l resins are expanding their applications from products such as adhesives, paints, ink binde.. |
|||
Molecular Weight | 20000 g/mol | 20000 g/mol | |
Unitika elitel UE3660 Polyester, Pellet High elongation type UE3600 PaintUNITIKA l resins are thermoplastic saturated copolymeric polyester resins. l resins are expanding their applications from products such as adhesives, paints, ink bi.. |
|||
Molecular Weight | 20000 g/mol | 20000 g/mol | |
Unitika elitel UE3700 Polyester, Pellet Hot melt adhesives, Adhesives for fibers, Adhesives for interlining clothsUNITIKA l resins are thermoplastic saturated copolymeric polyester resins. l resins are expanding their applications from p.. |
|||
Molecular Weight | 20000 g/mol | 20000 g/mol | |
Unitika elitel UE3800 Polyester, Pellet Hot melt adhesives, Adhesives for polyvinylchlorideUNITIKA l resins are thermoplastic saturated copolymeric polyester resins. l resins are expanding their applications from products such as adhesiv.. |
|||
Molecular Weight | 20000 g/mol | 20000 g/mol | |
Asahi Glass Lumiflon LF-302 Solvent Soluble Fluoropolymer w/ Melamine hardening agent Lumiflon was developed by Asahi Glass in 1982, and is unique being the first solvent soluble fluoropolymer. The FEVE based Lumiflon has a alternative copolymer. The complete inter-changeability betw.. |
|||
Molecular Weight | 20000 g/mol | 20000 g/mol | |
Unitika elitel UE3600 Polyester, Pellet High Tg, PET adhesiveness, Transparency, BinderUNITIKA l resins are thermoplastic saturated copolymeric polyester resins. l resins are expanding their applications from products such as adhesives, .. |
|||
Molecular Weight | 20000 - 60000 g/mol | 20000 - 60000 g/mol | |
Cathay Terryl® Renewable Engineering Polyamide Terryl® provides significant advantages in spinnability, dyeability, water absorption and comfort.Information provided by Cathay |