Unifrax Fiberfrax® Duraset® Flet

Category Ceramic , Oxide , Aluminum Oxide , Silicon Oxide
Manufacturer Unifrax I LLC
Trade Name Fiberfrax®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Unifrax Fiberfrax® Duraset® Flet.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Fiberfrax® Lo-Con™ felt and Duraset® flet are unique product forms in the Unifrax Corporation's extensive ceramic fiber product family. Felt products extend the performance of Fiberfrax papers in a product form with lower densities and increased mat thickness. Felt products are compressible but resilient; they conform to irregular surfaces yet have sufficient integrity to hold their shape in gaskets and formed parts. Both felt grades are wet laid, uniform, ceramic fiber mats which have been impregnated with a thermosetting resin. In Lo-Con flet, this resin has been precured to produce a semi-flexible rolled sheet. The binders in Duraset have been left uncured so they can be molded under heat and pressure to retain a complex shape after processing. The organic binders remain functional at low and moderate temperatures (to 650°F); however, the core ceramic fiber materials will provide consistent performance at temperatures well in excess of 2000°F, providing excellent thermal insulation in a wide range of applications.Fiberfax Duraset is a lightweight mat made from spun Fiberfrax ceramic fibers which have been impregnated with a thermosetting resin. Supplied in uncured form, it can be formed with the simultaneous application of pressure and heat to achieve complex shapes of rigid consistency for thermal and acoustical shielding. Use of Fiberfrax spun fibers allows for production of parts with severe draws without tearing during the forming process. Duraset flet is an excellent insulator with a high temperature use limit. If wet by water or steam, thermal and physical properties remain unaffected after drying. Duraset felt is unaffected by most chemicals except hydrofluoric and phosphoric acids and concentrated alkalies.Product AdvantagesFormabilityFlexibilityHigh temperature stabilityLow thermal conductivityLow heat storageWeight reductionThermal shock resistanceHigh heat reflectanceExcellent corrosion resistanceEasy to wrap, shape, and cutTypical ApplicationsAutomotive Exhaust Heat ShieldCommercial Fire Protection ApplicationsAerospace Heat ShieldingInformation Provided by Unifrax I LLC
Physical Properties Metric English Comments
Specific Gravity 2.73 g/cc
2.73 g/cc
Density 0.152 g/cc
0.00550 lb/in³
Nominal Core Density
Loss On Ignition 9.0 %
9.0 %
Thermal Properties Metric English Comments
Melting Point 1760 °C
3200 °F
Maximum Service Temperature, Air 1260 °C
2300 °F
Recommended Operating Temperature
Component Elements Properties Metric English Comments
Al2O3 40 - 45 %
40 - 45 %
SiO2 50 - 55 %
50 - 55 %
Processing Properties Metric English Comments
Cure Time 1.50 - 2.00 min

@Temperature 204 - 232 °C
0.0250 - 0.0333 hour

@Temperature 400 - 450 °F
Descriptive Properties Value Comments
Color Yellow/Tan
Fiber Index (% Wt) 70
Other Inorganics (%) <5
Temperature Grade (°C) 1260