Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melting Point = 1760 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 1760 °C
3200 °F
Pyrotek Grade 1250 Ceramic fiber paper
Pyrotek Grade 1250 ceramic fiber paper is manufactured under carefully controlled conditions from high purity fibers to ensure close thickness tolerance and uniformity of density. The product conta..
Melting Point 1760 °C
3200 °F
Pyrotek Pyrite Vacuum Formed Product
Off White ColorApplicationsTap hole cones Riser sleeves Launder insulation Head boxes Ladle lining Pouring cups AdvantagesGood thermal shock resistance High strength/weight ratio Low thermal conduct..
Melting Point 1760 °C
3200 °F
Mid-Mountain Materials HYTEX® 2200 Ceramic Fiber Industrial Textile
HYTEX® 2200 Ceramic Fiber Industrial Textiles are exceptionally effective high temperature textile products capable of withstanding continuous temperatures up to 2200ºF (1205ºC). Manufactur..
Melting Point 1760 °C
3200 °F
Thermal Ceramics 2600E RPC Shapes
RPC 2600 is an insulating material produced by blending alumina-silicate fibers and polycrystalline fibers with high purity silica binders. The alumina fibers form a matrix within the material, and ..
Melting Point 1760 °C
3200 °F
Thermal Ceramics 2800 RPC Shapes
RPC 2800 is an insulating material produced by blending alumina-silicate fibers and alumina fibers with high purity silica binders. The polycrystalline alumina fibers form a matrix within the materi..
Melting Point 1760 °C
3200 °F
Thermal Ceramics Cerachem Blanket
Cerachem Blanket is a 2600°F (1427°C) maximum temperature rated refractory blanket formed from a unique, patented, spun alumina-silica-zirconia fiber. It is specially designed for applications whe..
Melting Point 1760 °C
3200 °F
Thermal Ceramics Kao-Tex Cloth 2000
Insert Material- InconelKao-Tex 2000 textiles are made from alumina-silica ceramic fibers that are reinforced with an organic carrier fiber for added strength and stability, making them an excellent..
Melting Point 1760 °C
3200 °F
Thermal Ceramics Kaowool 2600 High Temperature Board
Kaowool 2600 using high alumina fibers along with Kaowool ceramic fibers is an excellent dimensional stable product at 2600°F (1427°C) where minimal shrinkages are very important.Applications: App..
Melting Point 1760 °C
3200 °F
Thermal Ceramics Kaowool 830 Millboard
Thermal Ceramics Kaowool Millboard products are processed from a slurry consisting of Kaowool ceramic fibers, fillers and binders. The fiber raw material is Kaolin, a naturally occurring high-purity..
Melting Point 1760 °C
3200 °F
Thermal Ceramics Kaowool Blanket, Blanket S Mesh Enclosed Rounds, Strips and Blankets
Kaowool ceramic fiber blankets can be encased in stainless steel wire meshes for many useful purposes. The wire mesh alloy used is determined by the atmosphere and temperature the enclosed product w..
Melting Point 1760 °C
3200 °F
Thermal Ceramics Kaowool Flex-Wrap Paper
Kaowool Flex-Wrap is produced from a blend of Kaowool high purity ceramic fibers and organic binders in a unique paper making process. Due to its low organic binder content, offgassing is at a minim..
Melting Point 1760 °C
3200 °F
Thermal Ceramics Kaowool PM Low Temperature Board
Kaowool PM is manufactured to close tolerances with an excellent surface finish. Kaowool PM has a good thermal conductivity and can easily be die-cut.Features: Excellent thermal conductivity Capabil..
Melting Point 1760 °C
3200 °F
Thermal Ceramics Kaowool S Blanket Strip
Thermal Ceramics Kaowool® Strip products are cut from either Kaowool Blanket, Blanket S, Cerablanket®, or Cerachem® Blanket. These products are available in many forms and lengths depending upon ..
Melting Point 1760 °C
3200 °F
Thermal Ceramics Kaowool Wet Felt
Thermal Ceramics Kaowool Wet Felt is manufactured by combining Kaowool ceramic fiber with an inorganic bonding agent. It is very pliable with good green strength. Wet Felt may be cut into any size o..
Melting Point 1760 °C
3200 °F
Thermal Ceramics K-Shield AG Felt
Meets BMS9-19 and AMS 3680 Rev. C specifications. K-Shield Felt products are produced from premium, cleaned Kaowool high-purity fibers and a special thermosetting binder system in a unique paper-mak..
Melting Point 1760 °C
3200 °F
Thermal Ceramics K-Shield Felt
K-Shield Felt products are produced from premium, cleaned Kaowool high-purity fibers and a special thermosetting binder system in a unique paper-making process. The cleaning process improves the the..
Melting Point 1760 °C
3200 °F
Thermal Ceramics K-Shield Felt AG/Min-K Composite
Thermal Ceramics has recently introduced a composite insulation system which combines the high temperature use limits of ceramic fiber felts with the low thermal conductivity benefits of microporous..
Melting Point 1760 °C
3200 °F
Thermal Ceramics Pyro-Bloc Burner Bloc
Features: Replaces dense castable burner blocksLightweight Excellent insulator/thermal shock resistant High mechanical abuse resistance Variety of sizes/attachment systems Low heat storage Cost effe..
Melting Point 1760 °C
3200 °F
Thermal Ceramics Pyro-Bloc C T-Bar Module
Features:Monolithic, edge-grained ceramic fiber module Available in uncompressed densities from 8 to 15 pcf (128 - 240 kg/m3)Easy access attachment allows quick installation over coated shells Insta..
Melting Point 1760 °C
3200 °F
Thermal Ceramics Pyro-Log R Fiber
Pyro-Log is an uncompressed monolithic mass of ceramic fiber. Pyro-Log fiber is available in 6" and 8" (152 mm to 203 mm) thicknesses with densities up to 15 pcf (240 kg/m3). Manufactured in three t..
Melting Point 1760 °C
3200 °F
Thermal Ceramics RPC™ 2300-W Wet Felt
Wet Felt is a high-alumina, ceramic fiber material made by a vacuum forming process that produces a unique insulating process capable of withstanding 2300°F (1260°C). Bonded with our standard bond..
Melting Point 1760 °C
3200 °F
Unifrax Fiberfrax® 7001-F-5 High Purity Bulk Fiber
Fiberfrax Bulk Fibers are manufactured to be used as feedstock in manufacturing processes or other applications where product consistency is critical. Manufactured on large, computer-controlled fur..
Melting Point 1760 °C
3200 °F
Unifrax Fiberfrax® Durablanket® 2600 Ceramic Fiber Insulator
Fiberfrax Durablanket 2600 insulation extends the high-temperature performance of the Durablanket product line. The product is made from high-purity alumina, zirconia, and silica spun ceramic fiber..
Melting Point 1760 °C
3200 °F
Unifrax Fiberfrax® Durablanket® S Ceramic Fiber Insulator
Fiberfrax Durablanket S insulation is a strong, lightweight, flexible needled blanket that is made from spun ceramic fibers. Available in a wide variety of thicknesses, widths and densities, Durabl..
Melting Point 1760 °C
3200 °F
Unifrax Fiberfrax® Duraboard® 350ES Ceramic Fiber Board
Fiberfrax® Duraboard® products are a family of rigid, high-temperature ceramic fiber boards manufactured in a wet forming process using Fiberfrax alumina-silica fibers and binders. All Duraboard ..
Melting Point 1760 °C
3200 °F
Chosun Refractories 1500 ACE BLANKET Blanket
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Melting Point 1760 °C
3200 °F
Thermal Ceramics Alfibond 2100 Shapes
Alfibond 2100 is a versatile and economical insulation made from kaolin-based alumina-silica fibers.Features: No organic binders Nominal 29 lb/ft3 (13 kg/m3) density ceramic fiber insulation Non we..
Melting Point 1760 °C
3200 °F
Thermal Ceramics Valcor® G-AZ
The Valcor line of fired refractory shapes, manufactured by Thermal Ceramics, has a proven track record in molten glass contact applications. The shapes are engineered to meet precise customer speci..
Melting Point 1760 °C
3200 °F
Unifrax Fiberfrax® Bulk 8000 AZS High-Temperature Fiber
In addition to Fiberfrax Bulk Fibers, Unifrax has the ability to produce many different specialty fibers that provide a variety of desirable performance properties for certain applications. These f..
Melting Point 1760 °C
3200 °F
Unifrax Fiberfrax® Duraset® Flet
Fiberfrax® Lo-Con™ felt and Duraset® flet are unique product forms in the Unifrax Corporation's extensive ceramic fiber product family. Felt products extend the performance of Fiberfrax papers i..
Copyright © lookpolymers.com All Rights Reserved