Total PPH 3662 Polypropylene Homopolymer, Fiber Grade, for Staple Fiber, Multifilament Yarns and Slit Tape

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Fiber Grade
Manufacturer Total Atofina
Trade Name PPH
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total PPH 3662 Polypropylene Homopolymer, Fiber Grade, for Staple Fiber, Multifilament Yarns and Slit Tape.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Fading Resistance TOTAL Polypropylene 3662 is formulated to resist gas fading while maintaining excellent processing stabilityProcess Stability. 3662 features excellent processability and the good physical properties necessary for fibers and multifilaments.FDA. 3662 complies with all applicable FDA regulations for food contact applications.Recommended Applications. TOTAL Polypropylene 3662 is recommended for staple fibers and bulk continuous filament (BCF) yarns.Information provided by Total Petrochemicals.
Physical Properties Metric English Comments
Specific Gravity 0.905 g/cc
0.905 g/cc
ASTM D1505
Melt Flow 10.2 g/10 min
10.2 g/10 min
ASTM D1238, L
Mechanical Properties Metric English Comments
Elongation at Yield 70 %
70 %
ASTM D3218
Tensile Modulus 1.79 GPa
260 ksi
ASTM D638
Tenacity 0.309 N/tex
3.50 g/denier
ASTM D3218
Flexural Modulus 1.655 GPa
240.0 ksi
ASTM D790
Flexural Stiffness 1310 MPa
190000 psi
ASTM D790
Thermal Properties Metric English Comments
Melting Point 165 °C
329 °F
DSC