Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melt Flow = 10.2 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 10.2 g/10 min

@Load 10.0 kg,
Temperature 220 °C
10.2 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
SABIC Innovative Plastics GELOY FXW750SK ASA+PC
Sparkle Metallic VisualFx ASA+PC Resin - Med. Heat & Impact Resin
Melt Flow 10.2 g/10 min

@Load 1.20 kg,
Temperature 300 °C
10.2 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
SABIC Innovative Plastics Lexan® FXD941A PC (Europe-Africa-Middle East)
Transparent/translucent PC for light diffusion special effects. Color package may affect performance.
Melt Flow 10.2 g/10 min

@Load 1.20 kg,
Temperature 300 °C
10.2 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
SABIC Innovative Plastics Lexan® FXM941A PC
PC in special effects colors. Metallic and pearlescent additives. Color package may affect performance.
Melt Flow 10.2 g/10 min

@Load 2.16 kg,
Temperature 190 °C
10.2 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Silon TA 2322 HD Blue Catalyst Masterbatch
Masterbatch for use with SILON Silane cross-linkable PE-Xb Compounds TA 1108 HD.TA 2322 HD, together with the above mentioned graft, contains the cross-linking catalyst to complete a Sioplas System...
Melt Flow 10.2 g/10 min
10.2 g/10 min
ASTM D1238, L
Total PPH 3662 Polypropylene Homopolymer, Fiber Grade, for Staple Fiber, Multifilament Yarns and Slit Tape
Fading Resistance TOTAL Polypropylene 3662 is formulated to resist gas fading while maintaining excellent processing stabilityProcess Stability. 3662 features excellent processability and the good..
Melt Flow 10.2 g/10 min

@Load 2.16 kg,
Temperature 190 °C
10.2 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Arkema Group Evatane® 1080 VN 5 Ethylene Vinyl Acetate
EVA copolymer made by high pressure tubular process. Applications Grade for molding very flexible articles. Examples: gaskets, medical.ISO data provided by the manufacturer, Arkema.
Copyright © lookpolymers.com All Rights Reserved