Total Finaprene® 435 Styrene-Butadiene TPE Copolymer Compounded to 54 MFI  (discontinued **)

Category Polymer , Thermoplastic , Elastomer, TPE , Styrenic TPE , Styrene-Butadiene
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total Finaprene® 435 Styrene-Butadiene TPE Copolymer Compounded to 54 MFI  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Styrene-Butadiene CopolymerDescription: Finaprene® is a thermoplastic elastomer type radial styrene-butadiene block copolymer. Thanks to its medium molecular weight, Finaprene® 435 provides excellent mechanical properties and abrasion resistance to the compound along with a good fluidity.Applications: Thanks to its very high crumb porosity Finaprene® 435 is designed for the compounding industry. This crumb shape, along with the medium molecular weight confer a quick and important oil absorption capacity to the polymer and lead to the production of high quality compounds with good MFI.Content of the compound for which the listed properties apply: F484: 105F435: 30Oil: 40GPPS: 20HIPS: 20CaCO3: 15Additional Notes: DIN Abrasion: 190 mm³Data provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics product lines.
Physical Properties Metric English Comments
Viscosity Measure 14 cSt
14 cSt
Toluene Solution; Finaprene 1008 Test
Melt Flow 54 g/10 min

@Load 5.00 kg,
Temperature 190 °C
54 g/10 min

@Load 11.0 lb,
Temperature 374 °F
Mechanical Properties Metric English Comments
Hardness, Shore A 55
55
Finaprene 1505 Test
Tensile Strength, Ultimate 5.30 MPa
769 psi
ASTM D638
Elongation at Break 520 %
520 %
ASTM D638
300% Modulus 0.00380 GPa
0.551 ksi
Tear Strength 22.2 kN/m
127 pli
Abrasion 190
190
mm³; DIN Abrasion