Polymer Property : Melt Flow = 54 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 54 g/10 min

@Load 10.0 kg,
Temperature 190 °C
54 g/10 min

@Load 22.0 lb,
Temperature 374 °F
ISO 1133
Multibase TPSiV® 4200-80A Thermoplastic Elastomer
FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; Good chemical resistanceAPPLICATIONS: Solution for soft touch overmolding on consumer e..
Melt Flow 54 g/10 min

@Load 5.00 kg,
Temperature 200 °C
54 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
PolyOne Dynaflex™ G7970-9 NSFG Thermoplastic Elastomer (TPE)
Dynaflex™ G7970-9 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,..
Melt Flow 54 g/10 min

@Load 5.00 kg,
Temperature 200 °C
54 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
PolyOne Dynaflex™ G7980-9 NSFG Thermoplastic Elastomer (TPE)
Dynaflex™ G7980-9 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,..
Melt Flow 54 g/10 min

@Load 5.00 kg,
Temperature 200 °C
54 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
PolyOne Dynaflex™ G7980-9001-02 Thermoplastic Elastomer (TPE)
Dynaflex™ G7980-9001-02 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropylen..
Melt Flow 54 g/10 min

@Load 5.00 kg,
Temperature 190 °C
54 g/10 min

@Load 11.0 lb,
Temperature 374 °F
Total Finaprene® 435 Styrene-Butadiene TPE Copolymer Compounded to 54 MFI  (discontinued **)
Styrene-Butadiene CopolymerDescription: Finaprene® is a thermoplastic elastomer type radial styrene-butadiene block copolymer. Thanks to its medium molecular weight, Finaprene® 435 provides excel..
Melt Flow 54 g/10 min

@Load 5.00 kg,
Temperature 200 °C
54 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
PolyOne Dynaflex™ G7970-9001-02 Thermoplastic Elastomer (TPE)
Dynaflex™ G7970-9001-02 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropylen..
Melt Flow 54 g/10 min

@Load 8.70 kg,
Temperature 190 °C
54 g/10 min

@Load 19.2 lb,
Temperature 374 °F
ASTM D1238
Lubrizol Estane® MVT 80AF3 Thermoplastic Polyurethane, Moisture Vapor Transmission
Type: Estane® MVT 80AF3 TPU is a aromatic polyether-based thermoplastic polyurethane (TPU).Features: High moisture vapor transmission, good low temperature properties and elasticity.Uses: Blown and..
Melt Flow 54 g/10 min

@Load 2.16 kg,
Temperature 230 °C
54 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
ExxonMobil PP7075L1 Polypropylene Impact Copolymer
Product Description: A nucleated impact copolymer resin with high flow and antistatic properties. It is suitable for molding applications like disposable houseware, consumer products, toys and rigi..