Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.00380 GPa | 0.551 ksi | ISO/R527 |
Polykemi AB POLYelast TPE E706 Thermoplastic Elastomer, EPDM-based Information provided by Polykemi AB |
|||
300% Modulus | 0.00380 GPa | 0.551 ksi | |
Total Finaprene® 435 Styrene-Butadiene TPE Copolymer Compounded to 79 MFI
(discontinued **) Styrene-Butadiene CopolymerDescription: Finaprene® is a thermoplastic elastomer type radial styrene-butadiene block copolymer. Thanks to its medium molecular weight, Finaprene® 435 provides excel.. |
|||
300% Modulus | 0.00380 GPa | 0.551 ksi | |
Total Finaprene® 435 Styrene-Butadiene TPE Copolymer Compounded to 54 MFI
(discontinued **) Styrene-Butadiene CopolymerDescription: Finaprene® is a thermoplastic elastomer type radial styrene-butadiene block copolymer. Thanks to its medium molecular weight, Finaprene® 435 provides excel.. |
|||
300% Modulus | 0.00380 GPa | 0.551 ksi | ISO 37 |
Huntsman AVALON® 60 AE-ESD Thermoplastic Polyurethane AVALON® ESD range are soft TPUs that deliver the improved bonding strength and mechanical properties required to produce high-quality footwear on roundtable machines – specifically safety sh.. |
|||
300% Modulus | 0.00380 GPa @Temperature 23.0 °C |
0.551 ksi @Temperature 73.4 °F |
12 months, Weathering @ 45° South, 12 mil - Black, Shelf |
Lubrizol Estane® 58610 Thermoplastic Polyurethane Features: Combines flexibility, toughness and excellent roll release for calendering and melt coating applications.Uses: Injection molding and general extrusion techniques. It is used in film, shee.. |
|||
300% Modulus | 0.00380 GPa | 0.551 ksi | |
Lubrizol ESTANE® 5703 Ester Based Thermoplastic Polyurethane Features: Soft compound with high elongation, displays low temperature flexibility and abrasion resistance. It can be processed by means of solution coating, extrusion and melt coating.Uses: Adhesiv.. |
|||
300% Modulus | 0.00380 GPa | 0.551 ksi | Vulcanizate, Press cured, TC95 +3min at 160°C |
Dow Nordel® IP 4520 Molded Golf Grip FormulationNordel® IP 4520 |
|||
300% Modulus | 0.00380 - 0.00920 GPa | 0.551 - 1.33 ksi | ASTM D 638 |
API Megol AM SV/P SEBS Adhesion Modified Overmolding for Polar Polymers Over-molding allows for the creation of composite finished products in a single phase, removing the need for successive gluing or mechanical fixing steps. This also reduces environmental impact as .. |