ThyssenKrupp 75Cr1 Saw Steel, Four-High Mill Plate

Category Metal , Ferrous Metal , Carbon Steel
Manufacturer ThyssenKrupp
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ThyssenKrupp 75Cr1 Saw Steel, Four-High Mill Plate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Heat treatment: tempered to max. 130ksiInformation Provided by Thyssen Krupp
Component Elements Properties Metric English Comments
Carbon, C 0.78 %
0.78 %
Chromium, Cr 0.40 %
0.40 %
Manganese, Mn 0.70 %
0.70 %
Silicon, Si 0.30 %
0.30 %