Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP THERMOCOMP PF00DS PA 6 (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOCOMP PF00DS PA 6 (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP THERMOCOMP* PF00DS is a compound based on PA6 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.
Physical Properties Metric English Comments
Density 1.70 g/cc
0.0614 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 235 MPa
34100 psi
5 mm/min; ISO 527
Elongation at Break 1.8 %
1.8 %
5 mm/min; ISO 527
Flexural Strength 335 MPa
48600 psi
2 mm/min; ISO 178
Flexural Modulus 19.0 GPa
2760 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 14.0 kJ/m²
6.66 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 65.0 kJ/m²
30.9 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 20.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
11.1 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 220 °C
428 °F
Edgew 120*10*4 sp=100mm; ISO 75/Ae
Flammability, UL94 HB

@Thickness 0.800 mm
HB

@Thickness 0.0315 in
UL 94 by SABIC-IP