Teknor Apex UNIPRENE® 7010-80 Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer Teknor Apex Company
Trade Name UNIPRENE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex UNIPRENE® 7010-80 Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Teknor Apex Company
Physical Properties Metric English Comments
Specific Gravity 0.960 g/cc
0.960 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 80
80
5 seconds; ASTM D2240
Tensile Strength, Yield 8.27 MPa
1200 psi
ASTM D412
Elongation at Break 400 %
400 %
ASTM D412
100% Modulus 0.00483 GPa
0.700 ksi
ASTM D412
Tear Strength 42.1 kN/m
240 pli
ASTM D624
Compression Set 31 %
31 %
23°C, 22 hr.; ASTM D395, Method B
52 %
52 %
100°C, 22 hr.; ASTM D395, Method B
Thermal Properties Metric English Comments
Brittleness Temperature <= -60.0 °C
<= -76.0 °F
ASTM D746