Teknor Apex Sinvicomp SIM 6019 Polyvinyl Chloride, Flexible

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Flexible Grade
Manufacturer Teknor Apex Company
Trade Name Sinvicomp
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex Sinvicomp SIM 6019 Polyvinyl Chloride, Flexible.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: Asia Pacific Features: High Strength Uses: Electrical/Electronic Applications < Forms: Pellets Processing Method: Injection MoldingInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.31 g/cc
1.31 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 76
76
ASTM D2240
Tensile Strength, Yield 7.4980 MPa
1087.5 psi
Change in tensile strength after 168 hours at 212°F; ASTM D638
10.0 MPa
1450 psi
9.8 in/min; ASTM D638
Elongation at Break 135 %
135 %
Change after 168 hours at 212°F; ASTM D638
180 %
180 %
9.8 in/min; ASTM D638
Thermal Properties Metric English Comments
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm

@Temperature 20.0 °C
1.00e+14 ohm-cm

@Temperature 68.0 °F
BS 2782