Material Notes:
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Film, Medical Applications Forms-PelletsInformation provided by Teknor Apex Company
Physical Properties Metric English Comments
Specific Gravity 1.24 g/cc
1.24 g/cc
23°C; ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 83
83
15 seconds; ASTM D2240
Tensile Strength at Break 20.0 MPa
2900 psi
ASTM D412
Tensile Strength, Yield 8.27 MPa
1200 psi
100%; ASTM D412
Elongation at Break 280 %
280 %
ASTM D412
Thermal Properties Metric English Comments
Brittleness Temperature -17.0 °C
1.40 °F
ASTM D746