Physical Properties Metric English Comments
Melt Flow 7.80 g/10 min

@Load 2.16 kg,
Temperature 230 °C
7.80 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Teknor Apex Flexalloy® 9604-75 Polyvinyl Chloride, Elastomer
Notes: 105°C Jacket; RoHS Compliant Features: Flame Retardant; High Heat Resistance; Low Temperature Flexibility; Sunlight Resistant (720 hours) Uses Cable Jacketing Wire Types: SEOW; SEW; SJEOW;..