Teknor Apex Fireguard® 910L16-C6-NL1 Polyvinyl Chloride, Flexible

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Flexible Grade , PVC, Wire and Cable Grade
Manufacturer Teknor Apex Company
Trade Name Fireguard®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex Fireguard® 910L16-C6-NL1 Polyvinyl Chloride, Flexible.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Notes: RoHS Compliant Features: Flame Retardant; Low Smoke Emission Uses: Plenum Cable Jacketing Wire Types: CL2P; CL3P; CMP; FPLP; MPP; OFNP Agency Ratings: NEC Article 725; NEC Article 760; NEC Article 770; NEC Article 800; UL 13; UL 1424; UL 1651; UL 444; UL QMTT2 .E200337 Processing Method: Extrusion Forms: Pellets Additional Notes: Dynamic Heat Stability at 205°C, 100 rpm, 72 gr. #5 Bowl (Minutes to Decomposition): 44 Kayness ACR at 370°F, 1000 sec-1: 424 Pa-s Peak Heat Release Rate: 111 kW/m2 Average Heat Release Rate: 67 kW/m2 Total Heat Released: 62 MJ/m2 Average Heat of Combustion: 12.54 MJ/kg Average Specification Extinction Area: 262 m2/kg Peak Smoke: 1.1 1/mInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.63 g/cc
1.63 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore C 81
81
10 seconds; ASTM D2240
88
88
ASTM D2240
Tensile Strength at Break 15.2 MPa
2200 psi
ASTM D638
Elongation at Break 200 %
200 %
ASTM D638
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 75.0 °C
167 °F
Continuous Use; ASTM D794
Brittleness Temperature -20.0 °C
-4.00 °F
ASTM D746
Oxygen Index 46 %
46 %
ASTM D2863
Electrical Properties Metric English Comments
Dielectric Constant 3.74

@Frequency 1.00e+6 Hz
3.74

@Frequency 1.00e+6 Hz
ASTM D150
4.75

@Frequency 1000 Hz
4.75

@Frequency 1000 Hz
ASTM D150
Dissipation Factor 0.037

@Frequency 1.00e+6 Hz
0.037

@Frequency 1.00e+6 Hz
ASTM D150
0.063

@Frequency 1000 Hz
0.063

@Frequency 1000 Hz
ASTM D150
Processing Properties Metric English Comments
Melt Temperature 193 °C
380 °F
Descriptive Properties Value Comments
Appearance Opaque