Material Notes:
Information provided by Teknor Apex Company
Physical Properties Metric English Comments
Specific Gravity 1.15 g/cc
1.15 g/cc
ASTM D792
Melt Flow 2.1 g/10 min

@Load 2.16 kg,
Temperature 230 °C
2.1 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 42
42
ASTM D2240
Tensile Strength, Yield 18.5 MPa
2680 psi
ASTM D412
Elongation at Break 490 %
490 %
ASTM D412
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 125 °C
257 °F
Continuous; UL-1581
Brittleness Temperature -56.0 °C
-68.8 °F
ASTM D746
Oxygen Index 23 %
23 %
ASTM D2863