Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | -56.0 °C | -68.8 °F | ASTM D746 |
PolyOne Synprene™ RT-5155 RoHS Natural Styrene Butadiene Block Copolymer (SBC) Synprene™ thermoplastic elastomers (TPEs) are compounds based on styrenic block copolymer (SBC) technology, and can be formulated to deliver extremely low hardness values not found in other elastom.. |
|||
Brittleness Temperature | -56.0 °C | -68.8 °F | ASTM D746 |
PolyOne Elastamax™ HTE 3070 Polyvinyl Chloride + NBR (PVC+NBR) Elastamax™ HTE Series thermoplastic elastomers (TPEs) are based upon compounded blends of PVC resins and nitrile rubber. These elastomeric materials provide outstanding resistance to hydrocarbons a.. |
|||
Brittleness Temperature | -56.0 °C | -68.8 °F | ASTM D746 |
PolyOne Elastamax™ HTE 3170 Polyvinyl Chloride + NBR (PVC+NBR) Elastamax™ HTE Series thermoplastic elastomers (TPEs) are based upon compounded blends of PVC resins and nitrile rubber. These elastomeric materials provide outstanding resistance to hydrocarbons a.. |
|||
Brittleness Temperature | -56.0 °C | -68.8 °F | Wide variability between samples is observed.; ASTM D746 |
DuPont Performance Polymers Hypalon® 40S Chlorosulfonated Polyethylene Rubber, Carbon Black Filled Compound
( Carbon black compound with 100 parts Hypalon; 27.8 parts sublimed litharge dispersion; 55 parts carbon black; 55 parts aromatic process oil; 0.5 parts MTBS; and 2 parts Tetrone® A rubber accelerato.. |
|||
Brittleness Temperature | <= -56.0 °C | <= -68.8 °F | TPE-0089 (ASTM D 746) |
Advanced Elastomer Systems Santoprene® 251-80 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic flame retardant elastomer with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonated polyethylene. It can b.. |
|||
Brittleness Temperature | <= -56.0 °C | <= -68.8 °F | TPE-0089 (ASTM D 746) |
Advanced Elastomer Systems Santoprene® 451-87 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic flame retardant wire and cable elastomer with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonated polyethy.. |
|||
Brittleness Temperature | -56.0 °C | -68.8 °F | |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with DOP Plasticizer MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Brittleness Temperature | -56.0 °C | -68.8 °F | ASTM D746 |
LyondellBasell Microthene® G MN71120 Low Density Polyethylene (Rotomolding) General DescriptionMicrothene G polyolefin powders are ground, irregularly-shaped particles designed for use in a broad range of specialty applications. Microthene G powders combine the unique prop.. |
|||
Brittleness Temperature | -56.0 °C | -68.8 °F | ASTM D746 |
Teknor Apex APEX® 1519-39 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMForms-PelletsFeatures- Good flexibility Information provided by Teknor Apex Company |
|||
Brittleness Temperature | -56.0 °C | -68.8 °F | ASTM D746 |
Teknor Apex APEX® 4167 Polyvinyl Chloride, Flexible Notes: 60°C Jacket; RoHS Compliant Features: High Gloss; Sunlight Resistant (720 hours)Uses: Flexible Cord Jacketing Forms: Pellets Wire Types: SJTW; STW; SJT; SRDT; ST; SVT Agency Ratings: UL QM.. |
|||
Brittleness Temperature | -56.0 °C | -68.8 °F | ASTM D746 |
Teknor Apex APEX® 77-W280B-9 Polyvinyl Chloride, Flexible Notes: 60°C Jacket; RoHS Compliant Uses: Wire and Cable ApplicationsForms: PelletsInformation Provided by Teknor Apex |
|||
Brittleness Temperature | -56.0 °C | -68.8 °F | ASTM D746 |
Teknor Apex ELEXAR® EL 8623 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Brittleness Temperature | -56.0 °C | -68.8 °F | |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with DOP Plasticizer MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Brittleness Temperature | -56.0 °C | -68.8 °F | ASTM D746 |
Colorite Polymers 7444D General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
Brittleness Temperature | -56.0 °C | -68.8 °F | ASTM D746 |
Colorite Polymers 7588 Non-Phthalate 88 Series Vinyl Compound Description: The Colorite 88 series is a family of vinyl non-toxic compounds formulated to provide excellent low temperature flexibility characteristics. These compounds are designed for outside doo.. |
|||
Brittleness Temperature | -56.0 °C | -68.8 °F | ASTM D 746 |
AlphaGary Evoprene™ GF 6257 Automotive Thermoplastic Elastomer Evoprene™ GF is a hydrogenated styrene block copolymer based thermoplastic elastomer created for the automotive industry. It is specially formulated to have very low fogging characteristics suitab.. |
|||
Brittleness Temperature | -56.0 °C | -68.8 °F | ASTM D746 |
PolyOne Synprene® RT-5155 Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerNaturalIgnition ResistantApplications:Multi-PurposeMarket:Building and ConstructionConsumer GoodsIndustrialProcessing Method:Injection Mo.. |