Teknor Apex APEX® 65008 Polyvinyl Chloride, Flexible

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Flexible Grade , PVC, Wire and Cable Grade
Manufacturer Teknor Apex Company
Trade Name APEX®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex APEX® 65008 Polyvinyl Chloride, Flexible.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Notes: 75°C Jacket; RoHS Compliant Uses: Wire and Cable ApplicationsForms: PelletsInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.58 g/cc
1.58 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore C 86
86
10 seconds; ASTM D2240
Tensile Strength at Break 19.3 MPa
2800 psi
ASTM D638
Elongation at Break 230 %
230 %
ASTM D638
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 75.0 °C
167 °F
Continuous Use; ASTM D794
Brittleness Temperature -10.0 °C
14.0 °F
ASTM D746
Oxygen Index 42 %
42 %
ASTM D2863
Electrical Properties Metric English Comments
Volume Resistivity 1.10e+12 ohm-cm
1.10e+12 ohm-cm
ASTM D257
Dielectric Constant 3.58

@Frequency 1.00e+6 Hz
3.58

@Frequency 1.00e+6 Hz
ASTM D150
4.52

@Frequency 1000 Hz
4.52

@Frequency 1000 Hz
ASTM D150
Dissipation Factor 0.036

@Frequency 1.00e+6 Hz
0.036

@Frequency 1.00e+6 Hz
ASTM D150
0.068

@Frequency 1000 Hz
0.068

@Frequency 1000 Hz
ASTM D150
Descriptive Properties Value Comments
Appearance Opaque
Users viewing this material also viewed the following: