Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Techmer ES Statiblend® TPU G/CF40 40% Glass/Carbon Filled

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Thermoplastic Polyurethane, Elastomer, Glass Filled
Manufacturer Techmer ES
Trade Name Statiblend®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES Statiblend® TPU G/CF40 40% Glass/Carbon Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Carbon Fiber, 40% Filler by WeightInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.50 g/cc
0.0542 lb/in³
ASTM D792
Water Absorption 0.20 %

@Time 86400 sec
0.20 %

@Time 24.0 hour
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell R 70
70
ASTM D785
Tensile Strength, Yield 79.3 MPa
11500 psi
ASTM D638
Elongation at Yield 15 %
15 %
ASTM D638
Flexural Yield Strength 95.1 MPa
13800 psi
ASTM D790
Flexural Modulus 2.65 GPa
385 ksi
ASTM D790
Izod Impact, Notched 5.07 J/cm

@Thickness 3.17 mm
9.50 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 21.6 µm/m-°C
12.0 µin/in-°F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 171 °C
340 °F
Unannealed; ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+10 ohm-cm
1.00e+10 ohm-cm
ASTM D257