Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Taiwan PU Corporation TPUI-E80 General Grade, Injection Molding Polyester Base TPU

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyester Grade
Manufacturer Taiwan PU Corporation
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Taiwan PU Corporation TPUI-E80 General Grade, Injection Molding Polyester Base TPU.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Thermoplastic Polyurethane (TPU), General Grade, Polyester Base, Injection MoldingInformation provided by Taiwan PU Corporation.
Mechanical Properties Metric English Comments
Hardness, Shore A 80
80
Tensile Strength at Break 31.38 MPa
4551 psi
Elongation at Break 800 %
800 %
100% Modulus 0.00540 GPa
0.783 ksi
300% Modulus 0.00780 GPa
1.13 ksi
Resilience 45
45
%, Impact Resilience
Taber Abrasion, mg/1000 Cycles 40
40
Processing Properties Metric English Comments
Feed Temperature 170 °C
338 °F
Middle Barrel Temperature 175 °C
347 °F
Compress zone
Front Barrel Temperature 180 °C
356 °F
Metering zone
Adapter Temperature 185 °C
365 °F
Die Temperature 185 °C
365 °F