Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : 100% Modulus = 0.783 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
100% Modulus 0.00540 GPa
0.783 ksi
Value at 50°C is 1.8 MPa; ASTM D412-80
DuPont Performance Polymers Hypalon® 45 Chlorosulfonated Polyethylene Rubber, Uncured Carbon Black Filled Compound &
Carbon black compound with 100 parts Hypalon; 100 parts carbon black; 4 parts magnesia; and 1.5 parts propylene glycol. Physical property data below (except mooney viscosity) are for uncured film. ..
100% Modulus 0.00540 GPa
0.783 ksi
ASTM D412
Mearthane Durethaneâ„¢ S DS-290A Solid Polyurethane Elastomer
TDI backbone: ester.Summary: Durethane S is a solid urethane elastomer. Formulations are individually compounded and tested to meet OEM requirements for durometer, tensile strength, tear strength, ..
100% Modulus 0.00540 GPa
0.783 ksi
Taiwan PU Corporation TPU-E85 General Grade, Extrusion Molding Polyester Base TPU
Thermoplastic Polyurethane (TPU), General Grade, Polyester Base, Extrusion MoldingInformation provided by Taiwan PU Corporation.
100% Modulus 0.00540 GPa
0.783 ksi
Taiwan PU Corporation TPU-EH80 High Hydrolysis Resistance, Extrusion Molding Polyether Base TPU
Thermoplastic Polyurethane (TPU), High Hydrolysis Resistance, Polyether Base, Extrusion MoldingInformation provided by Taiwan PU Corporation.
100% Modulus 0.00540 GPa
0.783 ksi
Taiwan PU Corporation TPUI-E80 General Grade, Injection Molding Polyester Base TPU
Thermoplastic Polyurethane (TPU), General Grade, Polyester Base, Injection MoldingInformation provided by Taiwan PU Corporation.
100% Modulus 0.00540 GPa
0.783 ksi
Taiwan PU Corporation TPUI-G85 High Wear Resistance, Injection Molding Polycaprolactone Base TPU
Thermoplastic Polyurethane (TPU), High Wear Resistance, Polycaprolactone Base, Injection MoldingInformation provided by Taiwan PU Corporation.
100% Modulus 0.00540 GPa
0.783 ksi
DIN 53504
Lubrizol ESTANE® 58300 Ether Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
100% Modulus 0.00540 GPa
0.783 ksi
DIN 53504
Lubrizol ESTANE® 5714F1 Ether Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
100% Modulus 0.00540 GPa
0.783 ksi
Colorite Polymers Vinylbond 95-950-70 PVC Compound
Description: Vinylbond 95-950 series compounds are flexible PVC alloys which are formulated specifically for the window market industry. These compounds offer excellent bonding characteristics to ri..
100% Modulus 0.00540 GPa
0.783 ksi
Cured 7 min at 177°C and Post Cured 2 hr at 232°C
DuPont Performance Polymers VTR 8600 (GF-S) Peroxide Cured Fluoroelastomer (FKM)  (discontinued **)
FormulationVTR-8600