Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 80 PHR Hi-Sil 243 LD Filler

Category Polymer , Thermoset , Polyester, TS , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 80 PHR Hi-Sil 243 LD Filler.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear strength, oil and fuel resistance, and ozone resistance. The life expectancy of urethane is often 5 times longer than other elastomers, thus saving material costs and downtime expense. One shortcoming of polyurethanes is loss of physical properties at temperatures over 180°F (82°C). MILLATHANE HT has overcome this weakness.FormulationMillathane HT100.0Zinc Stearate0.5MBTS4.0MBT2.0THANECURE® ZM1.0Sulfur1.5Hi-Sil 243 LD80All information provided by TSE Industries
Mechanical Properties Metric English Comments
Hardness, Shore A 97
97
Tensile Strength, Yield 18.1 MPa
2620 psi
Elongation at Yield 283 %
283 %
100% Modulus 0.0105 GPa
1.52 ksi
200% Modulus 0.01616 GPa
2.344 ksi
Tear Strength 71.4 kN/m
407 pli
Die C
Compression Set 78 %

@Temperature 70.0 °C,
Time 79200 sec
78 %

@Temperature 158 °F,
Time 22.0 hour
Processing Properties Metric English Comments
Cure Time 30.0 min

@Temperature 154 °C
0.500 hour

@Temperature 310 °F
Press cured
Users viewing this material also viewed the following: