Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 71.3 kN/m | 407 pli | Graves |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 75 PHR N650 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tear Strength | 71.4 kN/m | 407 pli | Die C |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 80 PHR Hi-Sil 243 LD Filler MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Tear Strength | 71.4 kN/m | 407 pli | Die C |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 80 PHR Hi-Sil 243 LD Filler MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Tear Strength | 71.3 kN/m | 407 pli | Graves |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 75 PHR N650 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |