Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polyplastic Armamid® PA6 GF 30 HS-901 Nylon, 30% Glass Filled

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 30% Glass Fiber Filled
Manufacturer Polyplastic Group
Trade Name Armamid®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyplastic Armamid® PA6 GF 30 HS-901 Nylon, 30% Glass Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Injection molding, heat stabilizedInformation provided by PolyPlastic Group.
Physical Properties Metric English Comments
Density 1.37 g/cc
0.0495 lb/in³
ISO 1183
Linear Mold Shrinkage <= 0.0020 cm/cm
<= 0.0020 in/in
Linear Mold Shrinkage, Flow 0.0010 - 0.0020 cm/cm
0.0010 - 0.0020 in/in
ISO 294-4
Linear Mold Shrinkage, Transverse 0.0060 - 0.0080 cm/cm
0.0060 - 0.0080 in/in
ISO 294-4
Ash 30 %
30 %
ISO 3451
Mechanical Properties Metric English Comments
Tensile Strength at Break 172 MPa
24900 psi
ISO 527-1/-2
Elongation at Break 4.9 %
4.9 %
ISO 527-1/-2
Tensile Modulus 9.70 GPa
1410 ksi
ISO 527-1/-2
Flexural Strength 240 MPa
34800 psi
ISO 178
Flexural Modulus 8.50 GPa
1230 ksi
ISO 178
Charpy Impact Unnotched 7.80 J/cm²

@Temperature 23.0 °C
37.1 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 1.00 J/cm²

@Temperature 23.0 °C
4.76 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 203 °C
397 °F
ISO 75-1/-2
Processing Properties Metric English Comments
Melt Temperature 280 - 290 °C
536 - 554 °F
Mold Temperature 80.0 °C
176 °F
Drying Temperature 85.0 °C

@Time 14400 - 21600 sec
185 °F

@Time 4.00 - 6.00 hour
Users viewing this material also viewed the following: