Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00427 GPa | 0.619 ksi | |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 30 PHR N330 (HAF) Filler MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
100% Modulus | 0.00427 GPa | 0.620 ksi | |
Shin-Etsu Silicones SFX-14032AU Fluorosilicone Elastomer Shincor SFX14032AU is normal 90 Durometer fluorosilicone compounds. It is designed to process well in molding applications. Product Features: Excellent fuel and solvent resistance.Usable over a broa.. |
|||
100% Modulus | 0.00427 GPa | 0.620 ksi | heat aged one week at 300ºF |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 40 PHR N330 (HAF) Black MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
100% Modulus | 0.00427 GPa | 0.620 ksi | |
Colorite Polymers 6511 Clear Extrusion Vinyl Compound Description: Clear non-toxic vinyl compounds are utilized by the health and medical industries for the extrusion of various components for the production of devices. The vinyl components used in pre.. |
|||
100% Modulus | 0.00427 GPa | 0.620 ksi | |
Colorite Polymers 6512 Clear Injection Molding Vinyl Compound Description: Clear non-toxic vinyl compounds are utilized by the health and medical industries for injection molding of various components such as drip chambers, connectors, valves, etc. The vinyl c.. |
|||
100% Modulus | 0.00427 GPa | 0.620 ksi | |
Colorite Polymers Self Frosting™ 6511SF Vinyl Compound Description: Colorite has developed a family of vinyl compounds to satisfy the needs of those who need a smooth, low gloss, low friction surface for the products that they produce. Historically, thi.. |
|||
100% Modulus | 0.00427 GPa | 0.620 ksi | heat aged one week at 300ºF |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 40 PHR N330 (HAF) Black MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
100% Modulus | 0.00427 GPa | 0.620 ksi | ASTM D638 |
Colorite Polymers 6534 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
100% Modulus | 0.00427 GPa | 0.619 ksi | |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 30 PHR N330 (HAF) Filler MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |