Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 1-D Heavy Oil Plasticizer

Category Polymer , Thermoset , Polyester, TS , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 1-D Heavy Oil Plasticizer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subjected to high wear in service. It has a unique combination of excellent properties, such as low temperature characteristics, and resistance to heat deterioration, ozone cracking, weathering and swelling in oils or solvents.FormulationMillathane CM 100.0N-330 Carbon Black30.01-D Heavy Oil15.0MBTS4.0MBT1.0Sulfur0.75CAYTUR 40.35Zinc Stearate0.50All information provided by TSE Industries
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
63
63
aged in air at 100ºC for 4 days
Tensile Strength, Yield 22.1 MPa
3200 psi
aged in air at 100ºC for 4 days
31.7 MPa
4600 psi
Elongation at Break 470 %
470 %
aged in air at 100ºC for 4 days
610 %
610 %
300% Modulus 0.00862 GPa
1.25 ksi
0.0124 GPa
1.80 ksi
aged in air at 100ºC for 4 days
Users viewing this material also viewed the following: