Material Notes:
TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all production and processing stages, strict final inspection, and clearly defined development processes.TIMREX Primary Synthetic Graphite shows unique properties thanks to the combination of a consistent purity, perfect crystalline structure and well defined texture.Tribological and mechanical properties:Medium toughnessGood lubrication propertiesAdvantages and applications: Low friction coefficientLow wear of the counterpart Good transfer-film formationHigh electrical conductivity Suitable for pitch-bonded and resin-bonded brushes Information provided by TIMCAL
Physical Properties Metric English Comments
Bulk Density 0.230 g/cc
0.00831 lb/in³
Scott, Typical
Particle Size 5.0 µm
5.0 µm
at a density of 1.81 g/cc, pressure at 2.5 t/cc
5.0 µm
5.0 µm
Springback 11.5%, pressure 0.477 t/cc
13 µm
13 µm
at a density of 1.90 g/cc, pressure at 2.5 t/cc
20 µm
20 µm
Springback 13%, pressure 0.477 t/cc
30.1 µm
30.1 µm
d90, Typical
29 - 33 µm
29 - 33 µm
d90, Guaranteed
45 µm
45 µm
at a density of 1.85 g/cc, pressure at 2.5 t/cc
75 µm
75 µm
at a density of 1.73 g/cc, pressure at 2.5 t/cc
75 µm
75 µm
Springback 17%, pressure 0.477 t/cc
Specific Surface Area 8.6 m²/g
8.6 m²/g
BET
Ash 0.030 %
0.030 %
Typical
<= 0.10 %
<= 0.10 %
Guaranteed
Electrical Properties Metric English Comments
Electrical Resistivity 1.55 ohm-cm
1.55 ohm-cm
particle size 80 um, pressure 2.5 t/cc
1.60 ohm-cm
1.60 ohm-cm
particle size 42 um, pressure 2.5 t/cc
1.80 ohm-cm
1.80 ohm-cm
particle size 15 um, pressure 2.5 t/cc
2.25 ohm-cm
2.25 ohm-cm
particle size 10 um, pressure 2.5 t/cc
Processing Properties Metric English Comments
Moisture Content 0.10 %
0.10 %
Typical
<= 0.50 %
<= 0.50 %
Guaranteed
Descriptive Properties Value Comments
Crystallinity, Lc >100 nm