Styrolution Absolan® 2500 SAN

Category Polymer , Thermoplastic , SAN Polymer
Manufacturer Styrolution
Trade Name Absolan®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Styrolution Absolan® 2500 SAN.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Absolac 2500 is a heat and chemical resistant gradeInformation provided by Styrolution
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
ISO 1183
Melt Flow >= 11 g/10 min

@Load 10.0 kg,
Temperature 220 °C
>= 11 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 800 MPa
116000 psi
ISO 527
Thermal Properties Metric English Comments
Vicat Softening Point 107 °C

@Load 5.10 kg
225 °F

@Load 11.2 lb
120°C/h; ASTM D 1525