Material Notes:
Applications: STRUKTOL VP 3622 is used where conventional epoxy systems and prepolymers are unable to satisfy the demands of for example impact, flexural and peel strength.Information provided by Struktol
Physical Properties Metric English Comments
Density 1.12 g/cc
0.0405 lb/in³
Viscosity 9500 cP

@Temperature 25.0 °C
9500 cP

@Temperature 77.0 °F
Dynamic
Chemical Properties Metric English Comments
Acid Value <= 1.0
<= 1.0
Processing Properties Metric English Comments
Shelf Life >= 12.0 Month
>= 12.0 Month
in original sealed containers at temperatures less than 40°C
Descriptive Properties Value Comments
Appearance Clear, slightly yellowish, liquid epoxy resin
Elastomer Content % 40 Polyether
Epoxy Equivalent Weight (g/Eq) 330
Resin-base of the prepolymer DGEBA