Physical Properties Metric English Comments
Density 1.438 g/cc
0.05195 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 84
84
ISO 868
Tensile Strength at Break 16.6 MPa
2410 psi
ISO R 527
Elongation at Break 308 %
308 %
ISO R 527