Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 16.6 MPa | 2410 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible 90252 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength at Break | 16.6 MPa | 2410 psi | ISO R 527 |
Stir SpA SG 88 OIL (PVC) Application: Extrusion insulating oil-proof sheath CEI 20-11 type R 2Information provided by STIR SpA |
|||
Tensile Strength at Break | 16.6 MPa | 2410 psi | |
Asahi Glass Fluon® RA3540 10% Carbon Fiber, 30% Bronze, PTFE Filled Compound Fluon®PTFE FC has improved creep and wear resistance. A wide range of fillers such as glass fiber, graphite, bronze, carbon fiber are available. Information provided by Asahi Glass Company, Inc. |